When the arc or burn-off characteristics are not smooth and difficult to handle. Can?t control where the puddle goes.
glossary
glossary
Alloy of a composition that solidifies at a lower temperature than the individual elements of the alloy and freezes or solidifies at a constant temperature to form a fine mixture crystals made up of two or more phases.
The mixture of chemicals, minerals and metallic alloys applied to the core wire. The coating controls the welding current, the welding position, and provides a shielding atmosphere, deoxidizers to clean the weld metal, and the welding slag that absorbs impurities from the weld metal. It also helps shape the weld bead and becomes an insulating blanket over the weld bead.
The ability of a material to become permanently deformed without failure.
The percentage of time during a time period that a power source can be operated at rated output without overheating. Based on a ten minute cycle.